Coupling a capacity fade model with machine learning for early prediction of the battery capacity trajectory

Published in Applied Energy, 2025

Graphical abstract for Coupling a capacity fade model with machine learning for early prediction of the battery capacity trajectory

Recommended citation: Tingkai Li, Jinqiang Liu, Adam Thelen, Ankush Mishra, Xiao-Guang Yang, Zhaoyu Wang, Chao Hu, "Coupling a capacity fade model with machine learning for early prediction of the battery capacity trajectory." Applied Energy, 2025.